From: Dave Jones (DAVERJ) [#23]
 5 Aug 2006
To: Rodney Gold (RODNEY_GOLD) [#22] 5 Aug 2006

Don't forget that if you've used the ferric to etch stainless that the ferric now contains a fair amount of chromium, since stainless has a high chromium content. Chomium is a toxic metal.

EDITED: 5 Aug 2006 by DAVERJ


From: Ward (STENSONENG) [#24]
 5 Aug 2006
To: jeff (JCHUMBLEY) [#8] 6 Aug 2006

It seems that a firm known as Port Engravers in West Sacramento used to do
stainless a few years ago. In fact they were listed in the 2003 SBC Business to Business
yellow pages - Phone 916-371-7317. Good Luck - Ward Stenson "never to old to learn"