Full Version: Dye Sub on Metal

From: RALLYGUY (RALLYGUY1) [#26]
 16 Oct 2006
To: Mike (MIKEN) [#25] 16 Oct 2006

Hi Mike,

Unisub is properly done at 400 degrees for 60 seconds through the back. Aluminum conducts heat very efficiently, and it works just as well front or back with the temps and times.....Adding a pad can change the times however....so that will have to be accounted for.....


From: Mike (MIKEN) [#27]
 16 Oct 2006
To: RALLYGUY (RALLYGUY1) [#26] 16 Oct 2006

Brian:
Thanks, I'm getting closer. Just need to tweak it a bit.

Show messages:  1-5  6-25  26-27