Full Version: 304 Stainless Steel

From: Harvey only (HARVEY-ONLY) [#9]
 12 Apr 2005
To: Zonas [#7] 12 Apr 2005

Antares makes a special spiral cutting bit for stainless steel. I have purchased one in .010, (I believe), and need to test it. It is supposed to be a great improvement.

 


From: Engravin' Dave (DATAKES) [#10]
 12 Apr 2005
To: JayBeeOz [#8] 12 Apr 2005

John,

I use that same process when drilling mounting holes through glass, using only water as the coolant. I can't believe I didn't think of it for metal engraving applications. Thanks for opening my closed mind a little bit further.


From: laserman (MIKEMAC) [#11]
 12 Apr 2005
To: Harvey only (HARVEY-ONLY) [#4] 12 Apr 2005

Harvey,

FWI

Thermark and Cermark are now the same Ferro Corp. just finished the purchase of Thermark. In fact the two companies started as one (Cerdec) and then split and now are back together again.

 