Full Version: Sublimation or OEM
From: Harvey only (HARVEY-ONLY) [#9]
12 Feb 2007
To: logojohn [#8] 20 Feb 2007
- Press temperature is varying.
- Press pressure is varying.
- Not enough pressure. Try a little more. Not too much more.
- The substrate may have some stuff on it. Even a hair of a smudge of adhesive from a peel off sheet will make a non-stick surface.
- The first piece needs about 5 seconds more than the rest.
Hope something here may be helpful.