There are a few possibilities to inconsistent results.

  • Press temperature is varying.
  • Press pressure is varying.
  • Not enough pressure. Try a little more. Not too much more.
  • The substrate may have some stuff on it. Even a hair of a smudge of adhesive from a peel off sheet will make a non-stick surface.
  • The first piece needs about 5 seconds more than the rest.


Hope something here may be helpful.