From: Mike (MIKEN) [#25]
16 Oct 2006
To: Harvey only (HARVEY-ONLY) [#24] 17 Oct 2006
I think you're right. I didn't try times longer than 60 seconds but there was consider ink left on the paper. Next time I'll extend it.
For sure I'm going to Unisub metal though.
From: RALLYGUY (RALLYGUY1) [#26]
16 Oct 2006
To: Mike (MIKEN) [#25] 16 Oct 2006
Hi Mike,
Unisub is properly done at 400 degrees for 60 seconds through the back. Aluminum conducts heat very efficiently, and it works just as well front or back with the temps and times.....Adding a pad can change the times however....so that will have to be accounted for.....
From: Mike (MIKEN) [#27]
16 Oct 2006
To: RALLYGUY (RALLYGUY1) [#26] 16 Oct 2006
Brian:
Thanks, I'm getting closer. Just need to tweak it a bit.