From: Harvey only (HARVEY-ONLY) [#14]
29 Sep 2005
To: jeffrey [#13] 30 Sep 2005
Great info to know.
From: laserman (MIKEMAC) [#15]
30 Sep 2005
To: ALL
Ferro has a solution strictly for anodized metals It is LMM - 6046 It is a yellow paste. We have tested it and are not extremely happy with the results. It works but it is not a consistent process It seemed to vary from part to part.
We tested this a while ago so they may have improved it by now.
From: LaserMike [#16]
1 Oct 2005
To: jeffrey [#13] 3 Oct 2005
No pre lasering needed, just apply the cermark direct and blast away! ;-)
-Mike
EDITED: 1 Oct 2005 by LASERMIKE
Show messages: All
1-13
14-16